Description:
The fiber resulting from peroxide degradation, is characterized by narrow molecular weight distribution, low ash content, and good spinnability. The final products are mainly used as materials in the areas of decoration and Medical Treatment & Public Health.
PP fiber grade is widely used in the production of Non-woven Clothing, Short Fibers, Ultra-fine Staple Fibers.
narrow molecular weight distribution, low ash content, good spinnability.
No. | Item | Unit | Quality Index | Typical Value |
---|---|---|---|---|
1 | MFR | g/10min | 37±7.0 | 36 |
2 | Tensile Strength at yield | MPa | ≥31.0 | 31.3 |
3 | Tensile strength at broken | MPa | ≥8.0 | 18.7 |
4 | Isotactic Index | MPa | ≥1200 | 1330 |
5 | Ash | % | ≤0.030 | 0.017 |
6 | Isotactic Index | % | ≥96.0 | 97.5 |